The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 28, 2019

Filed:

Aug. 18, 2014
Applicant:

Thyssenkrupp Steel Europe Ag, Duisburg, DE;

Inventors:

Brigitte Hammer, Voerde, DE;

Thomas Heller, Duisburg, DE;

Frank Hisker, Bottrop, DE;

Rudolf Kawalla, Bobritzsch, DE;

Grzegorz Korpala, Freiberg, DE;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C22C 38/34 (2006.01); C21D 6/00 (2006.01); C21D 8/02 (2006.01); C22C 38/42 (2006.01); C23C 30/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/16 (2006.01); C22C 38/18 (2006.01); C21D 7/10 (2006.01); C21D 9/00 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); C21D 6/004 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/0205 (2013.01); C21D 8/0221 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/16 (2013.01); C22C 38/18 (2013.01); C22C 38/34 (2013.01); C22C 38/42 (2013.01); C23C 30/005 (2013.01); C21D 7/10 (2013.01); C21D 9/0068 (2013.01); C21D 2211/001 (2013.01);
Abstract

A complexly formed steel component may have a tensile strength Rm of greater than 1200 MPa and an elongation at break A50 of greater than 6%. Example methods for producing such components comprise providing a flat steel product, which in addition to iron and unavoidable impurities, contains in percent by weight 0.10-0.60% C, 0.4-2.5% Si, up to 3.0% Al, 0.4-3.0% Mn, up to 1% Ni, up to 2.0% Cu, up to 0.4% Mo, up to 2% Cr, up to 1.5% Co, up to 0.2% Ti, up to 0.2% Nb, and up to 0.5% V. At least 10% by volume of a microstructure of the flat steel product may consist of residual austenite comprising globular residual austenite islands with a grain size of at least 1 μm. Before being cooled, the flat steel product may be heated to a forming temperature of 150-400° C. and formed into a component with a degree of forming that is at most equal to uniform elongation Ag.


Find Patent Forward Citations