The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 28, 2019

Filed:

Jul. 25, 2017
Applicant:

Schott Ag, Mainz, DE;

Inventors:

Ulf Dahlmann, Landshut, DE;

Sabine Pichler-Wilhelm, Landshut, DE;

Jens Suffner, Landshut, DE;

Assignee:

SCHOTT AG, Mainz, DE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
A61K 6/083 (2006.01); C08L 33/04 (2006.01); C03C 3/083 (2006.01); C03C 3/089 (2006.01); C03C 4/08 (2006.01); C03C 3/118 (2006.01); C03C 3/064 (2006.01); A61K 6/00 (2006.01); C03C 4/00 (2006.01);
U.S. Cl.
CPC ...
C03C 4/087 (2013.01); A61K 6/002 (2013.01); A61K 6/0005 (2013.01); A61K 6/0091 (2013.01); C03C 3/064 (2013.01); C03C 3/118 (2013.01); C03C 4/0021 (2013.01);
Abstract

The amorphous, or at least partially crystalline, glass-based joining material is suitable for high-temperature applications, particularly in fuel cells and/or sensors. In addition to SiOand BOas glass formers, the joining material similarly contains BaO and CaO, whereby the amount of AlOis limited. The joining material has a coefficient of linear thermal expansion of at least 7.0·10Kin a range of 20° C. to 300° C. The joining material can be used for joining ferritic high-grade steels and/or chromium-containing alloys and/or ceramics, such as stabilized zirconium oxide and/or aluminium oxide.