The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 21, 2019

Filed:

Nov. 28, 2011
Applicants:

Jun-ichi Takahashi, Ehime, JP;

Kazuhiro Mori, Ehime, JP;

Inventors:

Jun-ichi Takahashi, Ehime, JP;

Kazuhiro Mori, Ehime, JP;

Assignee:
Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C22B 7/00 (2006.01); H01M 10/54 (2006.01); C22B 4/00 (2006.01); C22B 21/00 (2006.01); H01M 10/0525 (2010.01);
U.S. Cl.
CPC ...
C22B 7/001 (2013.01); C22B 4/00 (2013.01); C22B 21/0069 (2013.01); H01M 10/54 (2013.01); H01M 10/0525 (2013.01); Y02P 10/212 (2015.11); Y02P 10/214 (2015.11); Y02W 30/84 (2015.05);
Abstract

Provided is a method for increasing the rate of recovery of valuable metals when waste batteries batteries are treated by a dry process. The valuable metal recovery method in the dry step Sincludes a melting step STincluding melting waste batteries to form a melt, a slag separation step STincluding separating slag from the melt, and an alloy separation step STincluding separating an alloy of valuable metals from the melt, wherein the slag has an aluminium oxide content of 20% by weight to less than 75% by weight and an iron content of 5% by weight to 40% by weight, calculated as metallic iron, and silicon oxide and calcium oxide are added as fluxes in the melting step STso that the slag can have a melting point of at least 1,500° C., preferably at most 1,650° C.


Find Patent Forward Citations