The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 14, 2019

Filed:

Jul. 15, 2014
Applicant:

Thyssenkrupp Steel Europe Ag, Duisburg, DE;

Inventors:

Maria Köyer, Dortmund, DE;

Sascha Sikora, Lünen, DE;

Janko Banik, Altena, DE;

Manuela Ruthenberg, Dortmund, DE;

Jennifer Schulz, Unna, DE;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/00 (2006.01); C21D 8/00 (2006.01); C21D 6/00 (2006.01); C21D 1/18 (2006.01); C23C 2/12 (2006.01); C23C 2/28 (2006.01); C23C 2/40 (2006.01); C23C 2/06 (2006.01); C22C 38/38 (2006.01); C22C 38/32 (2006.01); C22C 38/28 (2006.01); C22C 38/06 (2006.01); C22C 38/04 (2006.01); C22C 38/02 (2006.01); C22C 18/04 (2006.01); C22C 21/10 (2006.01); B32B 15/01 (2006.01); C23C 28/02 (2006.01); C23C 30/00 (2006.01); B32B 15/04 (2006.01); C23C 28/00 (2006.01); B32B 15/18 (2006.01); B32B 15/20 (2006.01); C22C 18/00 (2006.01); C22C 21/00 (2006.01); C23C 2/26 (2006.01); C22C 30/06 (2006.01); C22C 38/00 (2006.01); C22C 38/14 (2006.01); C22C 38/18 (2006.01);
U.S. Cl.
CPC ...
C21D 9/0068 (2013.01); B32B 15/012 (2013.01); B32B 15/013 (2013.01); B32B 15/04 (2013.01); B32B 15/043 (2013.01); B32B 15/18 (2013.01); B32B 15/20 (2013.01); C21D 1/18 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/005 (2013.01); C22C 18/00 (2013.01); C22C 18/04 (2013.01); C22C 21/00 (2013.01); C22C 21/10 (2013.01); C22C 30/06 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/14 (2013.01); C22C 38/18 (2013.01); C22C 38/28 (2013.01); C22C 38/32 (2013.01); C22C 38/38 (2013.01); C23C 2/06 (2013.01); C23C 2/12 (2013.01); C23C 2/26 (2013.01); C23C 2/28 (2013.01); C23C 2/40 (2013.01); C23C 28/02 (2013.01); C23C 28/021 (2013.01); C23C 28/025 (2013.01); C23C 28/321 (2013.01); C23C 30/00 (2013.01); C23C 30/005 (2013.01); Y10T 428/12757 (2015.01); Y10T 428/12799 (2015.01); Y10T 428/12937 (2015.01); Y10T 428/12944 (2015.01); Y10T 428/12951 (2015.01); Y10T 428/12958 (2015.01); Y10T 428/12972 (2015.01); Y10T 428/12979 (2015.01); Y10T 428/24967 (2015.01); Y10T 428/24975 (2015.01); Y10T 428/263 (2015.01); Y10T 428/264 (2015.01); Y10T 428/265 (2015.01);
Abstract

A steel component formed from a flat steel having a yield point of 150-1100 MPa and a tensile strength of 300-1200 MPa and coated with an anticorrosion coating of an alloy that includes 35-70% by weight aluminum, 35-60% by weight zinc, 0.1-10% by weight magnesium, up to 10% by weight Si, and up to 5% by weight Fe. A blank obtained from the flat steel product is heated to at least 800° C. and formed into the steel component. Alternatively, the steel component may be formed into the steel component first and then heated to at least 800° C. Regardless, the steel component may then be hardened by sufficiently rapid cooling the steel component from a sufficiently high temperature.