The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 07, 2019

Filed:

Jan. 24, 2014
Applicant:

Nok Corporation, Tokyo, JP;

Inventors:

Nobuaki Tanaka, Fukushima, JP;

Takeshi Sato, Fukushima, JP;

Katsumi Abe, Kanagawa, JP;

Assignee:

NOK Corporation, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
F02F 11/00 (2006.01); B32B 15/06 (2006.01); B32B 7/12 (2006.01); F16J 15/12 (2006.01); B32B 25/14 (2006.01); C09J 5/02 (2006.01); C23C 22/50 (2006.01); B32B 15/18 (2006.01); B32B 25/00 (2006.01);
U.S. Cl.
CPC ...
F02F 11/002 (2013.01); B32B 7/12 (2013.01); B32B 15/06 (2013.01); B32B 15/18 (2013.01); B32B 25/00 (2013.01); B32B 25/14 (2013.01); C09J 5/02 (2013.01); C23C 22/50 (2013.01); F16J 15/122 (2013.01); B32B 2250/02 (2013.01); B32B 2255/06 (2013.01); B32B 2255/20 (2013.01); B32B 2255/26 (2013.01); B32B 2255/28 (2013.01); B32B 2307/306 (2013.01); B32B 2307/714 (2013.01); B32B 2307/7265 (2013.01); B32B 2581/00 (2013.01); B32B 2605/08 (2013.01); C09J 2205/306 (2013.01); C09J 2400/163 (2013.01); C09J 2400/166 (2013.01); C09J 2421/006 (2013.01);
Abstract

A rubber-metal laminated gasket material comprising a metal plate, a surface treating agent layer, an adhesive layer, and a rubber layer, the layers being sequentially laminated on the metal plate; wherein the surface treating agent layer is formed by applying a surface treating agent so that the coating amount on one surface is 30 to 1,000 mg/m, and the surface treating agent is free from chromium, has a mixing ratio of 20 to 90 wt. % of a fluorine-free titanium compound and 10 to 80 wt. % of alumina, and has a metal titanium content of 1 to 20 wt. %. The rubber-metal laminated gasket material has excellent LLC resistance under high temperature conditions.


Find Patent Forward Citations