The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 07, 2019

Filed:

Sep. 09, 2015
Applicant:

Aleris Rolled Products Germany Gmbh, Koblenz, DE;

Inventors:

Steven Kirkham, Ransbach-Baumbach, DE;

Bernd Jacoby, Limburg, DE;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B23K 35/02 (2006.01); B23K 35/28 (2006.01); B32B 15/01 (2006.01); C22C 21/00 (2006.01); C22C 21/02 (2006.01); C22C 21/10 (2006.01); C22C 21/16 (2006.01); F28F 21/08 (2006.01); C22F 1/04 (2006.01); B23K 101/06 (2006.01);
U.S. Cl.
CPC ...
B23K 35/0238 (2013.01); B23K 35/0222 (2013.01); B23K 35/0233 (2013.01); B23K 35/0283 (2013.01); B23K 35/28 (2013.01); B23K 35/286 (2013.01); B23K 35/288 (2013.01); B32B 15/01 (2013.01); B32B 15/016 (2013.01); C22C 21/00 (2013.01); C22C 21/02 (2013.01); C22C 21/10 (2013.01); C22C 21/16 (2013.01); C22F 1/04 (2013.01); F28F 21/084 (2013.01); B23K 2101/06 (2018.08); F28F 21/089 (2013.01);
Abstract

A multi-layered brazing sheet material including an aluminum core alloy layer, a brazing clad layer material on one face of the core layer, an inter-layer between the core layer and brazing clad layer material, and a water-side layer on the other face of the core layer. The core layer made from aluminum alloy having, in wt. %, up to 0.6% Si, up to 0.45% Fe, 0.6% to 1.25% Cu, 0.6% to 1.4% Mn, 0.08% to 0.4% Mg, up to 0.2% Cr, up to 0.25% Zr, up to 0.2% Ti, up to 0.3% Zn, balance aluminum and impurities. The brazing layer made from aluminum alloy having 6% to 14% Si and up to 2% Mg, balance aluminum and impurities. The inter-layer made from 1xxx-series aluminum alloy. The water-side layer made from 3xxx-series aluminum alloy having 0.5% to 1.8% Mn and 1% to 3.5% Zn.