The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 07, 2019

Filed:

Aug. 17, 2016
Applicant:

The Boeing Company, Chicago, IL (US);

Inventor:

Ravi Verma, Chesterfield, MO (US);

Assignee:

THE BOEING COMPANY, Chicago, IL (US);

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
B23K 20/12 (2006.01); B23K 20/233 (2006.01); B23K 20/16 (2006.01); B23K 20/24 (2006.01); B23K 103/10 (2006.01); B23K 103/18 (2006.01); B23K 103/00 (2006.01); B23K 103/16 (2006.01); B23K 101/00 (2006.01); B23K 103/14 (2006.01); B23K 103/08 (2006.01);
U.S. Cl.
CPC ...
B23K 20/1275 (2013.01); B23K 20/122 (2013.01); B23K 20/126 (2013.01); B23K 20/127 (2013.01); B23K 20/128 (2013.01); B23K 20/1255 (2013.01); B23K 20/1265 (2013.01); B23K 20/16 (2013.01); B23K 20/233 (2013.01); B23K 20/2336 (2013.01); B23K 20/24 (2013.01); B23K 2101/006 (2018.08); B23K 2103/10 (2018.08); B23K 2103/14 (2018.08); B23K 2103/15 (2018.08); B23K 2103/172 (2018.08); B23K 2103/18 (2018.08); B23K 2103/52 (2018.08);
Abstract

A method for forming a metal matrix composite (MMC) structure includes forming an assembly including at least two blocks of a primary phase material sharing an interface at which a secondary phase material is disposed. The assembly has a length, a width, and a thickness. The method also includes clamping the assembly to at least one of urge the at least two blocks toward each other or maintain the at least two blocks at a predetermined position. Also, the method includes passing a rotating friction-stir pin along the interface from the front edge to the rear edge. The friction-stir pin has a mixing length extending at least the width of the assembly, and passing the friction-stir pin along the length of the assembly disperses the secondary phase material into the primary phase material and welds the at least two blocks together.