The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 30, 2019

Filed:

Jan. 15, 2013
Applicant:

Salzgitter Flachstahl Gmbh, Salzgitter, DE;

Inventors:

Thomas Schulz, Salzgitter, DE;

Andreas Wedemeier, Braunschweig, DE;

Wilfried Sprock, Braunschweig, DE;

Volker Flaxa, Salzgitter, DE;

Friedrich Luther, Hannover, DE;

Ingwer Denks, WolfenbĂĽttel, DE;

Sven Schulz, Lengede, DE;

Assignee:

SALZGITTER FLACHSTAHL GMBH, Salzgitter, DE;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 8/02 (2006.01); C22C 38/02 (2006.01); C21D 9/00 (2006.01); C21D 1/20 (2006.01); C22C 38/00 (2006.01); C22C 38/06 (2006.01); C22C 38/22 (2006.01); C22C 38/24 (2006.01); C22C 38/26 (2006.01); C22C 38/28 (2006.01); C22C 38/32 (2006.01); C22C 38/38 (2006.01); B62D 29/00 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0252 (2013.01); B62D 29/007 (2013.01); C21D 1/20 (2013.01); C21D 8/0263 (2013.01); C21D 8/0284 (2013.01); C21D 9/0068 (2013.01); C21D 9/0087 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/06 (2013.01); C22C 38/22 (2013.01); C22C 38/24 (2013.01); C22C 38/26 (2013.01); C22C 38/28 (2013.01); C22C 38/32 (2013.01); C22C 38/38 (2013.01); C21D 2211/002 (2013.01); C21D 2211/005 (2013.01); C21D 2211/008 (2013.01);
Abstract

In a process for producing a cold- or hot-rolled steel strip from an ultrahigh-strength multiphase steel having a particular composition the required multiphase microstructure is generated during continuous heat treatment. The cold- or hot-rolled steel strip is heated in the continuous heat treatment furnace to a temperature in the range from 700 to 950° C. and the heat-treated steel strip is subsequently cooled from the heat treatment temperature at a cooling rate of from 15 to 100° C./s to a first intermediate temperature of from 300 to 500° C. followed by cooling at a cooling rate of from 15 to 100° C./s to a second intermediate temperature of from 200 to 250° C.; the steel strip is subsequently cooled at a cooling rate of from 2 to 30° C./s in air to room temperature or the cooling at a cooling rate of from 15 to 100° C./s is maintained from the first intermediate temperature to room temperature.