The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 30, 2019

Filed:

Jul. 20, 2015
Applicant:

Soochow University, Suzhou, CN;

Inventors:

Xiao Lin, Suzhou, CN;

Lei Yang, Suzhou, CN;

Yanjie Bai, Suzhou, CN;

Huilin Yang, Suzhou, CN;

Assignee:

SOOCHOW UNIVERSITY, Suzhou, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08K 3/16 (2006.01); C08K 3/28 (2006.01); C08L 3/04 (2006.01); A61L 24/00 (2006.01); A61L 24/02 (2006.01); A61L 24/08 (2006.01); C08L 3/02 (2006.01); C09J 9/02 (2006.01); C09J 11/04 (2006.01); C09J 103/02 (2006.01); H01B 1/22 (2006.01); H05K 1/09 (2006.01); C09D 11/52 (2014.01); C08B 30/14 (2006.01); H05K 1/03 (2006.01);
U.S. Cl.
CPC ...
C08K 3/16 (2013.01); A61L 24/001 (2013.01); A61L 24/0042 (2013.01); A61L 24/02 (2013.01); A61L 24/08 (2013.01); C08B 30/14 (2013.01); C08K 3/28 (2013.01); C08L 3/02 (2013.01); C08L 3/04 (2013.01); C09D 11/52 (2013.01); C09J 9/02 (2013.01); C09J 11/04 (2013.01); C09J 103/02 (2013.01); H01B 1/22 (2013.01); H05K 1/092 (2013.01); C08K 2003/162 (2013.01); C08K 2003/164 (2013.01); C08K 2003/166 (2013.01); C08K 2003/168 (2013.01); C08K 2003/287 (2013.01); C08K 2201/001 (2013.01); C08L 2203/02 (2013.01); C08L 2203/20 (2013.01); C08L 2205/025 (2013.01); C08L 2205/03 (2013.01); H05K 1/0393 (2013.01); H05K 2201/0108 (2013.01); H05K 2201/0314 (2013.01);
Abstract

A preparation method of a conductive elastomer includes the following steps: (1) according to the mass percent of 20˜75%, dissolving the metallic salts into deionized water to form an electrolyte solution, wherein said metallic salts is either of magnesium nitrate, sodium nitrate, zinc nitrate, cesium nitrate, calcium nitrate, neodymium nitrate, aluminum nitrate, potassium nitrate, potassium chloride, magnesium chloride, calcium chloride, sodium chloride, zinc chloride, cesium chloride, aluminum chloride or their combinations; (2) according to the mass percent of 10˜40%, mixing starches into the electrolyte solution prepared in step (1), then at the temperature of 33˜120° C., stirring to gelatinize the starches, forming a viscous liquid; (3) standing the viscous liquid obtained in step (2) at 25˜90° C. for 10 min to 48 h to obtain the conductive elastomer.