The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 23, 2019

Filed:

Jul. 22, 2016
Applicant:

Toyota Jidosha Kabushiki Kaisha, Toyota-shi, Aichi-ken, JP;

Inventors:

Yuya Ishihara, Miyoshi, JP;

Akihiro Ochiai, Nisshin, JP;

Assignee:

TOYOTA JIDOSHA KABUSHIKI KAISHA, Toyota-shi, Aichi-ken, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 2/18 (2006.01); H01M 2/16 (2006.01); H01M 4/04 (2006.01); H01M 4/131 (2010.01); H01M 4/50 (2010.01); H01M 4/505 (2010.01); H01M 4/52 (2010.01); H01M 4/525 (2010.01); H01M 4/62 (2006.01); H01M 4/66 (2006.01); H01M 10/04 (2006.01); H01M 10/0525 (2010.01); H01M 10/42 (2006.01); H01M 4/36 (2006.01); H01M 10/052 (2010.01);
U.S. Cl.
CPC ...
H01M 2/18 (2013.01); H01M 2/1653 (2013.01); H01M 2/1673 (2013.01); H01M 2/1686 (2013.01); H01M 4/043 (2013.01); H01M 4/0404 (2013.01); H01M 4/131 (2013.01); H01M 4/502 (2013.01); H01M 4/505 (2013.01); H01M 4/523 (2013.01); H01M 4/525 (2013.01); H01M 4/623 (2013.01); H01M 4/625 (2013.01); H01M 4/661 (2013.01); H01M 10/0431 (2013.01); H01M 10/0525 (2013.01); H01M 10/4235 (2013.01); H01M 4/0435 (2013.01); H01M 4/366 (2013.01); H01M 10/052 (2013.01);
Abstract

A non-aqueous electrolyte secondary battery includes: a positive electrode plate; a negative electrode plate; and a separator disposed between the positive electrode plate and the negative electrode plate. The separator includes a porous resin layer. The porous resin layer is made of polyolefin having a melting point of 80° C. or more and 135° C. or less. At least one of the positive electrode plate and the negative electrode plate has a surface facing the porous resin layer. The surface forms a contact angle of 30° or more with a molten droplet of the polyolefin.