The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 23, 2019

Filed:

Nov. 30, 2015
Applicant:

The Nanosteel Company, Inc., Providence, RI (US);

Inventors:

Daniel James Branagan, Idaho Falls, ID (US);

Brian E. Meacham, Idaho Falls, ID (US);

Jason K. Walleser, Idaho Falls, ID (US);

Jikou Zhou, Pleasanton, CA (US);

Alla V. Sergueeva, Idaho Falls, ID (US);

Assignee:

The NanoSteel Company, Inc., Providence, RI (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 9/52 (2006.01); C22C 37/10 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/08 (2006.01); C22C 38/10 (2006.01); C22C 38/34 (2006.01); C22C 38/48 (2006.01); C22C 38/52 (2006.01); C22C 38/54 (2006.01); C22C 38/56 (2006.01); C22C 45/02 (2006.01);
U.S. Cl.
CPC ...
C22C 45/02 (2013.01); C21D 9/525 (2013.01); C22C 37/10 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/08 (2013.01); C22C 38/105 (2013.01); C22C 38/34 (2013.01); C22C 38/48 (2013.01); C22C 38/52 (2013.01); C22C 38/54 (2013.01); C22C 38/56 (2013.01);
Abstract

A method of forming an alloy composition including spinodal based glass matrix microconstituents. The method comprises melting an alloy composition comprising iron present in the range of 49 atomic percent (at %) to 65 at %, nickel present in the range of 10.0 at % to 16.5 at %, cobalt optionally present in the range of 0.1 at % to 12 at %, boron present in the range of 12.5 at % to 16.5 at %, silicon optionally present in the range of 0.1 at % to 8.0 at %, carbon optionally present in the range of 2 at % to 5 at %, chromium optionally present in the range of 2.5 at % to 13.35 at %, and niobium optionally present in the range of 1.5 at % to 2.5 at %, cooling the alloy composition at a rate of 10K/s to 10K/s.