The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 23, 2019

Filed:

Oct. 25, 2013
Applicants:

China Petroleum & Chemical Corporation, Beijing, CN;

China Petroleum & Chemical Corporation Exploration & Production Research Institute, Beijing, CN;

Inventors:

Changming Su, Beijing, CN;

Mengyun Zhao, Beijing, CN;

Jianzheng Su, Beijing, CN;

Rusheng Zhang, Beijing, CN;

Qiulian Long, Beijing, CN;

Suobing Zhang, Beijing, CN;

Danian Zhang, Beijing, CN;

Chenggang Zheng, Beijing, CN;

Yusheng Ma, Beijing, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09K 8/035 (2006.01); C08F 4/40 (2006.01); C08F 220/54 (2006.01); C08F 220/56 (2006.01); C09K 8/44 (2006.01); C08F 12/26 (2006.01); C08F 4/38 (2006.01); C09K 8/42 (2006.01); C09K 8/512 (2006.01);
U.S. Cl.
CPC ...
C08F 4/40 (2013.01); C08F 4/38 (2013.01); C08F 12/26 (2013.01); C08F 220/54 (2013.01); C08F 220/56 (2013.01); C09K 8/035 (2013.01); C09K 8/426 (2013.01); C09K 8/44 (2013.01); C09K 8/512 (2013.01);
Abstract

A cationic copolymer represented by the following formula (I) has a viscosity average molecular weight in a range from 2 million to 10 million. In the cationic copolymer, the mole fractions of three structural units corresponding to three monomers are as follows: x being in a range from 0.01 to 20%, y being in a range from 0 to 15%, and z=1−x−y. When used in the construction of leaking stoppage in an oil well, a cationic chemical lost circulation additive prepared with the cationic copolymer is mixed with an anionic drilling fluid in a section of the wellbore where lost circulation occurs. Then neutral reaction and cross linking reaction occur, so that the viscosity of the resulting mixture rapidly increases to form a space grid structure. This blocks off the leakage path, and thus effects on efficient leaking stoppage in a short time period.