The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 16, 2019

Filed:

Oct. 31, 2014
Applicants:

Compagnie Generale Des Etablissements Michelin, Clermont-Ferrand, FR;

Michelin Recherche ET Technique S.a., Granges-Paccot, CH;

Inventors:

Paul Winston, Greer, SC (US);

Xavier Saintigny, Greer, SC (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 9/06 (2006.01); B60C 1/00 (2006.01); C08L 9/00 (2006.01); C08K 3/04 (2006.01); C08K 3/06 (2006.01); C08K 5/14 (2006.01); C08L 57/02 (2006.01); C08K 5/00 (2006.01);
U.S. Cl.
CPC ...
C08L 9/06 (2013.01); B60C 1/0016 (2013.01); B60C 1/0025 (2013.01); C08K 3/04 (2013.01); C08K 3/06 (2013.01); C08K 5/0016 (2013.01); C08K 5/14 (2013.01); C08L 9/00 (2013.01); C08L 57/02 (2013.01); B60C 2200/14 (2013.01); C08L 2205/02 (2013.01);
Abstract

A rubber component for a tire is disclosed that is manufactured from a rubber composition that is based upon a cross-linkable elastomer composition that includes 100 phr of two elastomer types including at least 50 phr of a styrene-butadiene copolymer (SBR) with a polybutadiene (BR) as the remainder. Such compositions may further include between 75 phr and 130 phr of a carbon black. Also included in such elastomers is a plasticizing system that includes a plasticizing resin having a glass transition temperature (Tg) of at least 25° C. and a plasticizing liquid. The plasticizing system is added in an effective amount to provide the cured rubber composition with a shear modulus G* measured at 60° C. of between 0.7 MPa and 1.6 MPa and a measured Tg of between −30° C. and 0° C. The elastomer composition is cured with curing system that includes both a peroxide and sulfur.