The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 02, 2019

Filed:

Feb. 27, 2013
Applicant:

Salzgitter Flachstahl Gmbh, Salzgitter, DE;

Inventors:

Friedrich Luther, Hannover, DE;

Thomas Evertz, Peine, DE;

Stefan Muetze, Hannover, DE;

Michael Braun, Lehre, DE;

Assignee:

SALZGITTER FLACHSTAHL GMBH, Salzgitter, DE;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C21D 9/46 (2006.01); C23C 2/06 (2006.01); C23F 17/00 (2006.01); C21D 1/26 (2006.01); C21D 1/42 (2006.01); C21D 9/48 (2006.01); C21D 1/673 (2006.01); C21D 8/02 (2006.01); C23C 2/12 (2006.01);
U.S. Cl.
CPC ...
C21D 9/46 (2013.01); C21D 1/26 (2013.01); C21D 1/42 (2013.01); C21D 1/673 (2013.01); C21D 8/0226 (2013.01); C21D 8/0236 (2013.01); C21D 8/0263 (2013.01); C21D 9/48 (2013.01); C23C 2/06 (2013.01); C23C 2/12 (2013.01); C23F 17/00 (2013.01); C21D 2211/001 (2013.01); C21D 2211/008 (2013.01); Y02P 10/253 (2015.11);
Abstract

The invention relates to a method for producing a component from transformable steel by hot forming, in which a plate first is cut out of a strip or sheet as the pre-material, and is then heated to forming temperature and pre-formed, having an at least partially martensitic transformation structure after forming. Instead of a press mold hardening, the at least partially martensitic transformation structure is created in the pre-material, or in the plate to be formed, by austenitization and quenching already before forming, and then the thus-conditioned plate is reheated after forming, while maintaining the at least partially martensitic transformation structure, to a temperature below the Ac1 transformation temperature, and formed at this temperature.