The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 26, 2019

Filed:

Nov. 15, 2016
Applicant:

Denso-holding Gmbh & CO, Leverkusen, DE;

Inventors:

Thomas Markus Kaiser, Inden, DE;

Oleg Gryshchuk, Leverkusen, DE;

Assignee:

Denso-Holding GmbH & Co., Leverkusen, DE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C09J 9/00 (2006.01); B32B 7/14 (2006.01); B32B 1/08 (2006.01); B32B 25/16 (2006.01); B32B 25/02 (2006.01); B32B 25/08 (2006.01); B32B 15/06 (2006.01); B32B 15/18 (2006.01); C09J 7/30 (2018.01);
U.S. Cl.
CPC ...
C09J 9/00 (2013.01); B32B 1/08 (2013.01); B32B 7/14 (2013.01); B32B 15/06 (2013.01); B32B 15/18 (2013.01); B32B 25/02 (2013.01); B32B 25/08 (2013.01); B32B 25/16 (2013.01); C09J 7/30 (2018.01); B32B 2250/24 (2013.01); B32B 2270/00 (2013.01); B32B 2307/50 (2013.01); B32B 2307/714 (2013.01); B32B 2597/00 (2013.01); C09J 2409/00 (2013.01); C09J 2423/00 (2013.01);
Abstract

An anti-corrosion composition includes a first compound including: a first polyisobutylene having an average relative molar mass ranging from about 30,000 to about 100,000 g/mole and a Staudinger index ranging from about 15-70 cm/g, a first depolymerized butyl rubber with Brookfield viscosity at 66° C. ranging from about 400,000-2,000,000 mPa·s and an average molecular weight ranging from about 20,000-60,000, and combinations thereof. A second compound includes a second polyisobutylene having an average relative molar mass ranging from about 900,000-6,500,000 g/mole and a Staudinger index ranging from about 240-900 cm/g, at least one second partly cross-linked butyl rubber with a Mooney viscosity at 127° C. ranging from about 65-100 MU. The anti-corrosion composition includes at least one first or at least one second polyisobutylene as well as at least one first or at least one second butyl rubber.