The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 19, 2019

Filed:

Dec. 09, 2014
Applicant:

Hilti Aktiengesellschaft, Schaan, LI;

Inventors:

Ralf Meixner, Germaringen, DE;

Manfred Schallert, Nenzing, AT;

Michael Bischof, Bregenz, CH;

Jens Kondratiuk, Buchs/SG, CH;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B25D 17/08 (2006.01); B23K 1/00 (2006.01); C21D 1/60 (2006.01); B22D 25/02 (2006.01); C21D 9/00 (2006.01);
U.S. Cl.
CPC ...
B25D 17/088 (2013.01); B22D 25/02 (2013.01); B23K 1/0008 (2013.01); C21D 1/60 (2013.01); C21D 9/0068 (2013.01); B25D 2250/071 (2013.01); B25D 2250/075 (2013.01); B25D 2250/231 (2013.01); B25D 2250/301 (2013.01);
Abstract

A production method for a tool socket includes forming a hollow spindle An elongated recess is provided in the wall. The spindle includes unalloyed or low-alloyed steel grades. An insert includes a high-alloyed tool steel. The insert has a pedestal that is complementary to the recess and it also has a rib. The insert is placed into the hollow spindle in such a way that the pedestal rests in the recess and the rib projects into the interior of the spindle. The pedestal is soldered into the recess at a temperature that is above the Ac3 temperatures of the steel grades employed. The combined structure is cooled and then undergoes a heat treatment in an atmosphere containing sufficient carbon to carburize the hollow spindle but not sufficient to carburize the insert. The heat treatment of the combined structure is carried out at a temperature between 800° C. and 950° C. The combined structure is cooled down in a salt bath or liquid bath subsequent to the heat treatment.