The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 05, 2019

Filed:

May. 29, 2015
Applicant:

Menicon Co., Ltd., Nagoya-shi, Aichi, JP;

Inventors:

Eri Ito, Kasugai, JP;

Katsuhiro Yamamoto, Nagoya, JP;

Assignee:

MENICON CO., LTD., Nagoya, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 283/12 (2006.01); C08F 290/06 (2006.01); G02C 7/04 (2006.01); B29D 11/00 (2006.01); G02B 1/04 (2006.01); B29K 83/00 (2006.01); B29K 105/00 (2006.01);
U.S. Cl.
CPC ...
C08F 283/12 (2013.01); B29D 11/00134 (2013.01); C08F 290/06 (2013.01); G02B 1/043 (2013.01); G02C 7/04 (2013.01); B29K 2083/00 (2013.01); B29K 2105/0058 (2013.01);
Abstract

A contact lens is provided as hydrate of a copolymer of at least three components including (I) both terminal-polymerizable silicone oligomer exhibiting viscosity of at least 200 mPa·s at room temperature, (II) a hydrophilic monomer component having ethylenically unsaturated group, and (III) a hydrophobic monomer component having molecular weight of at most 700, wherein the lens exhibits an elastic-modulus ratio determined as ratio of a rupture elastic modulus to an initial elastic modulus in range of 0.8-1.2. The contact lens is transparent and by combination of high oxygen permeability and balance between softness and mechanical properties. The lens is produced through a process including steps of stirring material-liquid including at least three components of the above-mentioned (I), (II) and (III) under stirring power of 5-10000 W/m3 per unit volume of the material-liquid for at least 10 minutes, and injecting stirred material-liquid into a lens mold to polymerize material-liquid.