The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 26, 2019

Filed:

Oct. 29, 2015
Applicants:

Alm Holding Company, Onalaska, WI (US);

Ergon Asphalt & Emulsions, Inc., Jackson, MS (US);

Inventors:

Gerald H. Reinke, La Crosse, WI (US);

Gaylon L. Baumgardner, Jackson, MS (US);

Steven L. Engber, Onalaska, WI (US);

Assignees:

A.L.M. Holding Company, Onalaska, WI (US);

Ergon Asphalt & Emulsion, Inc., Jackson, MS (US);

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C08L 95/00 (2006.01); C04B 26/26 (2006.01); E01C 7/26 (2006.01); C08K 5/00 (2006.01); E01C 19/08 (2006.01); E01C 19/10 (2006.01); C09D 195/00 (2006.01); C08K 5/17 (2006.01); C04B 111/00 (2006.01); C08K 5/521 (2006.01);
U.S. Cl.
CPC ...
C08L 95/00 (2013.01); C04B 26/26 (2013.01); C08K 5/0008 (2013.01); C09D 195/00 (2013.01); E01C 7/265 (2013.01); E01C 19/08 (2013.01); E01C 19/10 (2013.01); C04B 2111/0075 (2013.01); C08K 5/17 (2013.01); C08K 5/521 (2013.01); C08L 2555/24 (2013.01); C08L 2555/34 (2013.01); C08L 2555/40 (2013.01); C08L 2555/60 (2013.01); C08L 2555/80 (2013.01); Y02A 30/333 (2018.01); Y02W 30/95 (2015.05);
Abstract

The present invention provides an asphalt paving composition including an essentially water-free, non-foamed warm mix asphalt binder composition modified with lubricating antistrip additives that can be mixed with uncompacted aggregate to provide a warm mix paving composition of the aggregate adequately coated with the essentially water-free, non-foamed binder and lubricating antistrip additive. This warm mix paving composition may be mixed at temperatures of 280° F. or lower and may be compacted at temperatures of 260° F. or lower that are below mixing and compacting temperatures of similar paving compositions that do not contain the disclosed lubricating antistrip additives.