The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 05, 2019

Filed:

Nov. 18, 2015
Applicant:

Diamond Innovations, Inc., Worthington, OH (US);

Inventors:

Jacob Palmer, Westerville, OH (US);

Lawrence Dues, Dublin, OH (US);

Rui Shao, Dublin, OH (US);

Gerold Weinl, Alvsjo, SE;

Assignee:

Diamond Innovations, Inc., Worthington, OH (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/58 (2006.01); C04B 35/5831 (2006.01); C04B 35/626 (2006.01); C04B 35/63 (2006.01); C04B 35/645 (2006.01);
U.S. Cl.
CPC ...
C04B 35/5831 (2013.01); C04B 35/6261 (2013.01); C04B 35/6264 (2013.01); C04B 35/6303 (2013.01); C04B 35/645 (2013.01); C04B 2235/386 (2013.01); C04B 2235/3847 (2013.01); C04B 2235/3886 (2013.01); C04B 2235/402 (2013.01); C04B 2235/405 (2013.01); C04B 2235/5436 (2013.01); C04B 2235/5445 (2013.01); C04B 2235/5472 (2013.01); C04B 2235/656 (2013.01); C04B 2235/80 (2013.01);
Abstract

Multi-step milling processes to prepare cBN composite powder forms a first powder mixture by adding a binder and a first cBN component, mills the first powder mixture for a first time period, combines a second cBN component with the milled first powder mixture to form a second powder mixture, and mills the second powder mixture for a second time period (less than the first time period) to form the cBN composite powder. A ratio of the D50 value of the second cBN component to the D50 value of the first cBN component is at least 3.0. Two-step milling with different milling times for the two cBN component fractions controls the amount of mill debris in the cBN composite powder mixture. Further processing of the cBN composite powder under HPHT conditions forms a cBN-based ceramic with an average value of a cBN particle free diameter of less than 2.0 microns.