The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 22, 2019

Filed:

Mar. 06, 2014
Applicants:

Thyssenkrupp Steel Europe Ag, Duisburg, DE;

Thyssenkrupp Rasselstein Gmbh, Andernach, DE;

Inventors:

Erhard Holleck, Duisburg, DE;

Eberhard Sowka, Dinslaken, DE;

Burkhard Kaup, Andernach, DE;

Stephan Schiester, Andernach, DE;

Assignees:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 8/04 (2006.01); C21D 9/48 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22B 9/04 (2006.01); C22B 9/10 (2006.01); B22D 11/00 (2006.01); B22D 11/113 (2006.01); B22D 11/116 (2006.01); B21B 1/22 (2006.01); B22D 11/12 (2006.01); B22D 11/126 (2006.01); B22D 11/14 (2006.01); C21D 1/26 (2006.01); C21D 6/00 (2006.01); C22C 38/00 (2006.01); C22C 38/06 (2006.01); C25D 5/36 (2006.01); B21B 1/46 (2006.01); B21D 35/00 (2006.01); B21D 51/26 (2006.01);
U.S. Cl.
CPC ...
C21D 8/0436 (2013.01); B21B 1/22 (2013.01); B22D 11/1206 (2013.01); B22D 11/126 (2013.01); B22D 11/14 (2013.01); C21D 1/26 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 8/041 (2013.01); C21D 8/0426 (2013.01); C21D 8/0463 (2013.01); C22B 9/04 (2013.01); C22B 9/10 (2013.01); C22C 38/001 (2013.01); C22C 38/004 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C25D 5/36 (2013.01); B21B 1/46 (2013.01); B21D 35/005 (2013.01); B21D 51/26 (2013.01);
Abstract

A method is disclosed for the operationally reliable production of a cold-rolled flat steel product of ≤0.5 mm in thickness for deep-drawing and ironing applications. In the method, a steel melt which (in wt %) comprises up to 0.008% C, up to 0.005% Al, up to 0.043% Si, 0.15-0.5% Mn, up to 0.02% P, up to 0.03% S, up to 0.020% N and in each case optionally up to 0.03% Ti and up to 0.03% Nb and, as a remainder, iron and unavoidable impurities, is, with the omission of a Ca treatment, subjected to a secondary metallurgical treatment which, in addition to a vacuum treatment, comprises a ladle furnace treatment and during which the steel melt to be treated is kept under a slag, the Mn and Fe contents of which are, in sum total, <15 wt %. From the steel melt, a thin slab or a cast strip are produced, which are subsequently hot-rolled to form a hot strip with a thickness of <2.5 mm and wound to form a coil. Subsequently, the hot strips are cold-rolled to form a flat steel product of up to 0.5 mm in thickness.