The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 15, 2019

Filed:

Apr. 19, 2012
Applicants:

Yoshitsugu Tatsuzawa, Tokyo, JP;

Hideki Fujii, Tokyo, JP;

Tomonori Kunieda, Tokyo, JP;

Kazuhiro Takahashi, Tokyo, JP;

Inventors:

Yoshitsugu Tatsuzawa, Tokyo, JP;

Hideki Fujii, Tokyo, JP;

Tomonori Kunieda, Tokyo, JP;

Kazuhiro Takahashi, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22D 7/00 (2006.01); C22F 1/18 (2006.01); B22D 11/00 (2006.01); B22D 21/00 (2006.01); B22D 30/00 (2006.01); C22C 14/00 (2006.01);
U.S. Cl.
CPC ...
C22F 1/183 (2013.01); B22D 7/005 (2013.01); B22D 11/001 (2013.01); B22D 21/005 (2013.01); B22D 30/00 (2013.01); C22C 14/00 (2013.01);
Abstract

A titanium slab for hot rolling comprised of a titanium slab obtain by smelting commercially pure titanium, wherein even if the breakdown process is omitted, the strip shaped coil after hot rolling is excellent in surface properties and a method of smelting that titanium slab are provided. The titanium slab according to the present invention is a titanium slab for hot rolling obtained by smelting commercially pure titanium including the β phase stabilizing element Fe, wherein the formation of coarse β phases is suppressed by making the average Fe concentration down to 10 mm from the surface layer of the surface which corresponds to at least the rolling surface of the titanium slab 0.01 mass % or less. A titanium slab obtained by smelting commercially pure titanium can be obtained by cooling until the surface becomes the β transformation point or less, then reheating it to the β transformation point or more, and gradually cooling from the slab surface layer.


Find Patent Forward Citations