The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 08, 2019

Filed:

Feb. 28, 2014
Applicant:

Jfe Steel Corporation, Tokyo, JP;

Inventors:

Yusuke Fushiwaki, Tokyo, JP;

Yoshiyasu Kawasaki, Tokyo, JP;

Yasunobu Nagataki, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C23C 2/02 (2006.01); C23C 2/06 (2006.01); C23C 2/28 (2006.01); C21D 9/46 (2006.01); C22C 18/00 (2006.01); C22C 38/06 (2006.01); C22C 38/60 (2006.01); C21D 1/76 (2006.01); B32B 15/01 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/08 (2006.01); C22C 38/12 (2006.01); C22C 38/14 (2006.01); C22C 38/16 (2006.01); C22C 38/18 (2006.01); C21D 1/26 (2006.01); C21D 6/00 (2006.01); C22C 38/38 (2006.01); C23F 17/00 (2006.01); C25F 1/06 (2006.01);
U.S. Cl.
CPC ...
C23C 2/02 (2013.01); B32B 15/013 (2013.01); C21D 1/26 (2013.01); C21D 1/76 (2013.01); C21D 6/001 (2013.01); C21D 6/002 (2013.01); C21D 6/005 (2013.01); C21D 6/008 (2013.01); C21D 9/46 (2013.01); C22C 18/00 (2013.01); C22C 38/002 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/12 (2013.01); C22C 38/14 (2013.01); C22C 38/16 (2013.01); C22C 38/18 (2013.01); C22C 38/38 (2013.01); C22C 38/60 (2013.01); C23C 2/06 (2013.01); C23C 2/28 (2013.01); C23F 17/00 (2013.01); C25F 1/06 (2013.01);
Abstract

Provided is a high-strength steel sheet that has good chemical convertibility and good corrosion resistance after electro deposition painting despite high Si and Mn contents. Also provided are a method for producing the high-strength steel sheet, a high-strength galvanized steel sheet formed by using the high-strength steel sheet, and a method for producing the high-strength galvanized steel sheet. A steel sheet containing, in terms of % by mass, C: 0.03 to 0.35%, Si: 0.01 to 0.50%, Mn: 3.6 to 8.0%, Al: 0.001 to 1.00%, P≤0.10%, S≤0.010%, and the balance being Fe and unavoidable impurities is annealed under condition under which a dew point of an atmosphere in a temperature zone of 550° C. or higher and A° C. or lower (A is a particular value that satisfies 600≤A≤750) inside an annealing furnace is controlled to −40° C. or lower.


Find Patent Forward Citations