The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 11, 2018

Filed:

Feb. 09, 2018
Applicant:

Fuji Xerox Co., Ltd., Tokyo, JP;

Inventors:

Kana Yoshida, Kanagawa, JP;

Masataka Kuribayashi, Kanagawa, JP;

Masahiro Uchida, Kanagawa, JP;

Takafumi Koide, Kanagawa, JP;

Yusuke Fukuda, Kanagawa, JP;

Katsuyuki Kitajima, Kanagawa, JP;

Koji Funaba, Kanagawa, JP;

Satomi Hara, Kanagawa, JP;

Assignee:

FUJI XEROX CO., LTD., Minato-ku, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
G03G 15/20 (2006.01); G03G 9/08 (2006.01); G03G 9/087 (2006.01);
U.S. Cl.
CPC ...
G03G 15/2089 (2013.01); G03G 9/081 (2013.01); G03G 9/0819 (2013.01); G03G 9/0827 (2013.01); G03G 9/08755 (2013.01); G03G 15/2017 (2013.01); G03G 2215/2009 (2013.01); G03G 2215/2016 (2013.01);
Abstract

An image forming apparatus includes an image holding member, a charging unit, an electrostatic charge image forming unit, a developing unit, a transfer unit, a fixing unit including a fixing belt, a pressurizing rotator that forms a nip by pressurizing an outer peripheral surface of the fixing belt, a sliding member that slides on an inner peripheral surface of the fixing belt in the nip, and a pressing member that presses the fixing belt in the direction of the pressurizing rotator, wherein a toner to be used includes a binder resin containing an amorphous resin and a crystalline resin and has specific physical properties described in the specification, and paraffin wax having a melting temperature of 60° C. to 80° C., and an absolute value of a difference between the melting temperature of the crystalline resin and the melting temperature of the paraffin wax is 10° C. or less.