The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 04, 2018

Filed:

Nov. 10, 2017
Applicant:

Kobe Steel, Ltd., Kobe-shi, JP;

Inventors:

Narikazu Hashimoto, Shimonoseki, JP;

Takahiro Shikama, Shimonoseki, JP;

Tsunetake Tsuyoshi, Shimonoseki, JP;

Assignee:

KOBE STEEL, LTD., Kobe-shi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22F 1/053 (2006.01); C22C 21/10 (2006.01);
U.S. Cl.
CPC ...
C22F 1/053 (2013.01); C22C 21/10 (2013.01);
Abstract

An aluminum alloy member resistant to cracking and having high strengths and excellent stress corrosion cracking resistance is manufactured by crushing a 7xxx aluminum alloy extrudate. Specifically, a 7xxx aluminum alloy extrudate containing Zn of 3.0-8.0%, Mg of 0.4-2.5%, Cu of 0.05-2.0%, and Ti of 0.005-0.2%, in mass percent, and prepared through press quenching is subjected to a reversion treatment, to crushing within 72 hours after the reversion treatment, and then to aging. The reversion treatment includes heating at a temperature rise rate of 0.4° C./second or more, holding in a temperature range of 200-550° C. for longer than 0 second, and cooling at a rate of 0.5° C./second or more. The ratio of the tensile residual stress σto the 0.2% yield stress σafter aging and the total content X of Mg and Zn satisfy a condition specified by Expression (1):≤−0.1+1.4  (1).