The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 27, 2018

Filed:

Sep. 27, 2013
Applicant:

Sumitomo Metal Mining Co., Ltd., Tokyo, JP;

Inventors:

Katsuya Kase, Ehime, JP;

Yasutaka Kamata, Ehime, JP;

Kazuomi Ryoshi, Ehime, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/525 (2010.01); C01G 53/00 (2006.01); B01J 19/24 (2006.01); H01M 4/04 (2006.01); H01M 10/0525 (2010.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/525 (2013.01); B01J 19/24 (2013.01); C01G 53/00 (2013.01); C01G 53/006 (2013.01); C01G 53/42 (2013.01); C01G 53/66 (2013.01); H01M 4/049 (2013.01); H01M 10/0525 (2013.01); B01J 2219/00033 (2013.01); B01J 2219/24 (2013.01); C01P 2004/51 (2013.01); C01P 2004/61 (2013.01); C01P 2006/11 (2013.01); H01M 2004/028 (2013.01);
Abstract

To improve cycling characteristics of a non-aqueous electrolyte secondary battery by obtaining a nickel-cobalt composite hydroxide having a sharp particle size distribution as a precursor, a slurry including a nickel-cobalt composite hydroxide obtained by continuously supplying an aqueous solution that includes at least nickel and cobalt, an ammonium ion donor aqueous solution and a caustic alkali aqueous solution to a reaction vessel and reacting, is continuously extracted and separated into a large particle size portion and s small particle size portion by classification, and the small particle size portion is continuously returned to the reaction vessel. As a result, a nickel-cobalt composite hydroxide is obtained that is expressed by the general formula: NiCoM(OH)(where, 0.05≤x≤0.50, 0≤y≤0.10, 0.05≤x+y≤0.50, and M is at least one kind of metal element selected from among Al, Mg, Mn, Ti, Fe, Cu, Zn and Ga, and that satisfies the relationships (D50−D10)/D50≤0.30, and (D90−D50)/D50≤0.30 among D10, D50 and D90 of this composite hydroxide.