The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 20, 2018

Filed:

Aug. 13, 2013
Applicant:

Nippon Light Metal Company, Ltd., Tokyo, JP;

Inventors:

Atsushi Oota, Aichi, JP;

Fumio Otake, Aichi, JP;

Takeshi Handa, Shizuoka, JP;

Assignee:
Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C22F 1/047 (2006.01); C22C 21/08 (2006.01); B32B 15/00 (2006.01); C22C 21/00 (2006.01); C22F 1/04 (2006.01); C23C 18/12 (2006.01); C23C 22/66 (2006.01); B32B 15/04 (2006.01); C25D 11/04 (2006.01); C25D 11/06 (2006.01); C25D 11/08 (2006.01); C25D 11/14 (2006.01); C25D 11/16 (2006.01); C22C 21/06 (2006.01); C22F 1/00 (2006.01); C25D 11/24 (2006.01);
U.S. Cl.
CPC ...
C22C 21/00 (2013.01); B32B 15/04 (2013.01); C22C 21/06 (2013.01); C22C 21/08 (2013.01); C22F 1/04 (2013.01); C22F 1/047 (2013.01); C23C 18/12 (2013.01); C23C 18/1216 (2013.01); C23C 22/66 (2013.01); C25D 11/04 (2013.01); C25D 11/06 (2013.01); C25D 11/08 (2013.01); C25D 11/14 (2013.01); C25D 11/16 (2013.01); C22F 1/00 (2013.01); C25D 11/246 (2013.01); Y10T 428/1259 (2015.01); Y10T 428/1266 (2015.01); Y10T 428/12597 (2015.01); Y10T 428/12604 (2015.01); Y10T 428/12611 (2015.01); Y10T 428/12618 (2015.01); Y10T 428/12667 (2015.01); Y10T 428/12736 (2015.01); Y10T 428/12764 (2015.01); Y10T 428/12993 (2015.01);
Abstract

An aluminum alloy sheet which is high in strength and excellent in heat conductivity, and which can be given an anodic oxide coating with a white color and a suitable yellowishness is provided. An aluminum alloy ingot containing Mg: 0.80 to 1.8 mass %, Fe: 0.05 to 0.30 mass %, Si: 0.20 mass % or less, Cu: 0.03 to 0.15 mass %, Mn: 0.05 to 0.20 mass %, and Cr: 0.05 to 0.15 mass %, restricts Zn to less than 0.15 mass %, and balance of Al and unavoidable impurities is treated by holding it at 560 to 620° C. for 1 to 5 hours, then hot rolled and, either through or not through process annealing, and cold rolled by a final cold rolling reduction of 15 to 95% to obtain an aluminum alloy sheet which has a 0.2% yield strength of 180 MPa or more and a conductivity of 40 (IACS %) or more.