The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 20, 2018

Filed:

Dec. 16, 2014
Applicant:

Dow Global Technologies Llc, Midland, MI (US);

Inventors:

Michael D. Read, Midland, MI (US);

Santosh S. Bawiskar, Freeport, TX (US);

Assignee:

Dow Global Technologies LLC, Midland, MI (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08K 5/14 (2006.01); C08F 255/02 (2006.01); C08K 5/092 (2006.01);
U.S. Cl.
CPC ...
C08F 255/02 (2013.01); C08K 5/092 (2013.01); C08K 5/14 (2013.01);
Abstract

The invention provides a process to form a 'functionalized ethylene-based polymer' from an ethylene-based polymer and at least one polar compound, said process comprising thermally treating a composition comprising the ethylene-based polymer, the at least one polar compound, and at least one peroxide, in at least one extruder comprising at least one barrel, to form a polymer melt; and wherein the at least one peroxide has a half life, at the maximum barrel temperature of the at least one extruder, of less than of the minimum residence time of the polymer melt in the at least one extruder. The invention further provides a composition comprising at least the following: a) an ethylene-based polymer comprising a melt viscosity, at 350° F. (177° C.), less than 50.000 cP, and b) at least one peroxide comprising a half-life from 0.10 to 2.00 minutes, at a temperature from 160° C. to 190° C.