The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 06, 2018

Filed:

Oct. 21, 2014
Applicant:

Uop Llc, Des Plaines, IL (US);

Inventors:

Nick J. Schoenfeldt, Chicago, IL (US);

David Stickley, Lombard, IL (US);

Jaime G. Moscoso, Mt. Prospect, IL (US);

Deng-Yang Jan, Elk Grove Village, IL (US);

Benjamin Daniel Yuhas, Evanston, IL (US);

Assignee:

UOP LLC, Des Plaines, IL (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 29/85 (2006.01); C07C 1/20 (2006.01); C01B 39/54 (2006.01); B01J 29/06 (2006.01); C01B 37/08 (2006.01); C01B 39/02 (2006.01); B01J 35/02 (2006.01);
U.S. Cl.
CPC ...
B01J 29/85 (2013.01); B01J 29/06 (2013.01); C01B 37/08 (2013.01); C01B 39/026 (2013.01); C01B 39/54 (2013.01); C07C 1/20 (2013.01); B01J 35/023 (2013.01); B01J 2229/12 (2013.01); B01J 2229/186 (2013.01); B01J 2229/34 (2013.01); B01J 2229/38 (2013.01); C07C 2529/85 (2013.01); Y02P 20/52 (2015.11); Y02P 30/42 (2015.11);
Abstract

Zeolitic materials with modified surface composition, crystal structure, crystal or particle size, and/or porosity, methods for making the same, and methods for converting oxygenates to olefins using the same are provided herein. In an exemplary embodiment, a method for reducing a surface silicon content of a silicon-containing zeolitic material is provided that includes providing a silicon-containing zeolitic material; and contacting the silicon-containing zeolitic material with a modifying solution comprising one or more of an amine, an alcoholamine, and an amino acid. In this embodiment, the contacting occurs under conditions suitable for the modifying solution to reduce a surface silicon content, increase the porosity, and/or decrease an average crystal or particle size of the silicon-containing zeolitic material.


Find Patent Forward Citations