The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 23, 2018

Filed:

Feb. 02, 2018
Applicant:

Guangdong Silver Age Sci & Tech Co., Ltd, Dongguan, Guangdong, CN;

Inventors:

Chunze Yan, Hubei, CN;

Yusheng Shi, Hubei, CN;

Yi Fu, Hubei, CN;

Yunsong Shi, Hubei, CN;

Teng Pan, Hubei, CN;

Yan Wang, Hubei, CN;

Qingsong Wei, Hubei, CN;

Jie Liu, Hubei, CN;

Assignee:

Other;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
A61F 2/00 (2006.01); C08G 65/40 (2006.01); C08K 3/32 (2006.01); C08L 61/16 (2006.01); B29C 64/153 (2017.01); B22F 3/105 (2006.01); B29B 13/06 (2006.01); B29B 13/10 (2006.01); C08G 65/46 (2006.01); B29K 71/00 (2006.01);
U.S. Cl.
CPC ...
C08G 65/4012 (2013.01); B22F 3/1055 (2013.01); B29B 13/06 (2013.01); B29B 13/10 (2013.01); B29C 64/153 (2017.08); C08G 65/46 (2013.01); C08K 3/32 (2013.01); C08L 61/16 (2013.01); B29K 2071/00 (2013.01); C08G 2650/40 (2013.01); C08K 2003/325 (2013.01); C08K 2201/005 (2013.01);
Abstract

The present invention discloses polyetheretherketone/nano-hydroxyapatite (PEEK/NANO-HA) composites for selective laser sintering (SLS), and a preparation method thereof. The method for preparing the composites comprises steps of: selecting PEEK having a particle size of 10-100 μm, and an aqueous solution of reaction precursorand an aqueous solution of reaction precursor, uniformly dispersing the PEEK in the aqueous solution of reaction precursor, adding the aqueous solution of reaction precursordropwise in the mixed solution of the aqueous solution of reaction precursorand the PEEK while stirring to adjust pH of the mixed solution to 10-12, and continuously reacting or 24-48 hours. The composites obtained by the preparation method of the present invention have the advantages of good biocompatibility, homogeneous morphology and good fluidity, and are advantageous to the powdering and shaping process during SLS.