The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 09, 2018

Filed:

Nov. 30, 2015
Applicant:

Hitachi Chemical Company, Ltd., Tokyo, JP;

Inventors:

Daisuke Fukae, Matsudo, JP;

Hideaki Kawata, Matsudo, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22C 38/18 (2006.01); C22C 38/22 (2006.01); C22C 38/34 (2006.01); C22C 38/36 (2006.01); C22C 38/02 (2006.01); C22C 30/00 (2006.01); C22C 1/05 (2006.01); B22F 5/00 (2006.01); C22C 1/08 (2006.01); C22C 1/10 (2006.01); C22C 33/02 (2006.01);
U.S. Cl.
CPC ...
C22C 38/36 (2013.01); B22F 5/009 (2013.01); C22C 1/05 (2013.01); C22C 1/08 (2013.01); C22C 1/10 (2013.01); C22C 30/00 (2013.01); C22C 33/0207 (2013.01); C22C 33/0285 (2013.01); C22C 38/02 (2013.01); C22C 38/22 (2013.01); C22C 38/34 (2013.01); B22F 2998/10 (2013.01);
Abstract

A sintered alloy having superior heat resistance and superior wear resistance and also having corrosion resistance against salt damage that may occur in cold-weather regions, and a production method therefor, are provided. The sintered alloy consists of, by mass %, 32.4 to 48.4% of Cr, 2.9 to 10.0% of Mo, 0.9 to 2.9% of Si, 0.3 to 1.8% of P, 0.7 to 3.9% of C, and the balance of Fe and inevitable impurities, and it has a density ratio of not less than 90% and includes carbides that are dispersed in a matrix of a metallic structure thereof.