The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 11, 2018

Filed:

Dec. 25, 2013
Applicants:

Ningxia Orient Tantalum Industry Co., Ltd., Shizuishan, Ningxia, CN;

National Engineering Research Center for Special Metal Materials of Tantalum and Niobium, Shizuishan, Ningxia, CN;

Inventors:

Guoqi Yang, Shizuishan, CN;

Aiguo Zheng, Shizuishan, CN;

Xueqing Chen, Shizuishan, CN;

Fukun Lin, Shizuishan, CN;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 15/02 (2006.01); H01G 9/042 (2006.01); B22F 9/04 (2006.01); H01G 9/15 (2006.01); B22F 1/00 (2006.01); H01G 9/052 (2006.01); H01G 9/04 (2006.01);
U.S. Cl.
CPC ...
H01G 9/042 (2013.01); B22F 1/0007 (2013.01); B22F 9/04 (2013.01); H01G 9/052 (2013.01); H01G 9/0525 (2013.01); H01G 9/15 (2013.01); B22F 2009/043 (2013.01); B22F 2999/00 (2013.01); H01G 2009/05 (2013.01); Y10T 428/12014 (2015.01); Y10T 428/12028 (2015.01); Y10T 428/12035 (2015.01); Y10T 428/12181 (2015.01);
Abstract

A method for providing a tantalum powder with a piece+block structure, comprising the following steps: 1) providing a granulous tantalum powder, and dividing same into a first part and a second part; 2) putting the first part of the tantalum powder in a ball mill for ball milling, taking the powder out after the ball milling and sieving same, and obtaining a tantalum powder in the form of a piece; 3) mixing the tantalum powder in the form of a piece and the second part of the tantalum powder to obtain a mixture, and preferably, the mixing proportion of the tantalum powder in the form of a piece and the granulous tantalum powder being 1:0.1˜1, preferably being 1:0.25˜0.8, and more preferably being 1:0.4˜0.6; and 4) performing the steps of water washing, acid washing, and nodularization on the mixture to finally obtain a tantalum powder with a piece+block structure.