The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 14, 2018

Filed:

Mar. 26, 2013
Applicants:

Sumitomo Electric Industries, Ltd., Osaka-shi, Osaka, JP;

Kyoto University, Kyoto-shi, Kyoto, JP;

Inventors:

Chihiro Hiraiwa, Itami, JP;

Masatoshi Majima, Itami, JP;

Atsushi Yamaguchi, Itami, JP;

Naho Mizuhara, Itami, JP;

Tetsuya Uda, Kyoto, JP;

Yohei Noda, Kyoto, JP;

Assignees:

Sumitomo Electric Industries, Ltd., Osaka-shi, Osaka, JP;

Kyoto University, Kyoto-shi, Kyoto, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 8/12 (2016.01); H01M 8/1253 (2016.01); C04B 35/48 (2006.01); H01M 4/90 (2006.01); H01B 1/12 (2006.01); C04B 35/486 (2006.01); C04B 35/626 (2006.01); H01M 4/88 (2006.01); H01M 8/124 (2016.01);
U.S. Cl.
CPC ...
H01M 8/1253 (2013.01); C04B 35/48 (2013.01); C04B 35/486 (2013.01); C04B 35/6261 (2013.01); H01B 1/122 (2013.01); H01M 4/881 (2013.01); H01M 4/8882 (2013.01); H01M 4/8889 (2013.01); H01M 4/9025 (2013.01); H01M 4/9033 (2013.01); H01M 8/12 (2013.01); C04B 2235/3215 (2013.01); C04B 2235/3225 (2013.01); C04B 2235/761 (2013.01); C04B 2235/786 (2013.01); C04B 2235/9607 (2013.01); H01M 2008/1293 (2013.01); H01M 2300/0071 (2013.01); Y02E 60/525 (2013.01); Y02P 70/56 (2015.11);
Abstract

Provided is a solid electrolyte laminate comprising a solid electrolyte layer having proton conductivity and a cathode electrode layer laminated on one side of the solid electrolyte layer and made of lanthanum strontium cobalt oxide (LSC). Also provided is a method for manufacturing the solid electrolyte. This solid electrolyte laminate can further comprise an anode electrode layer made of nickel-yttrium doped barium zirconate (Ni—BZY). This solid electrolyte laminate is suitable for a fuel cell operating in an intermediate temperature range less than or equal to 600° C.