The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 14, 2018

Filed:

Aug. 26, 2014
Applicant:

Nippon Steel & Sumitomo Metal Corporation, Tokyo, JP;

Inventors:

Naotsugu Yoshida, Kimitsu, JP;

Hirofumi Nakamura, Kimitsu, JP;

Takayuki Kamimura, Takarazuka, JP;

Nobuo Otsuka, Nishinomiya, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/16 (2006.01); C22C 38/08 (2006.01); C22C 38/02 (2006.01); C22C 38/06 (2006.01); B22D 11/00 (2006.01); C22C 38/00 (2006.01); C22C 38/04 (2006.01); C21D 9/00 (2006.01);
U.S. Cl.
CPC ...
B22D 11/00 (2013.01); B22D 11/001 (2013.01); C21D 9/0081 (2013.01); C22C 38/00 (2013.01); C22C 38/002 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/16 (2013.01); C21D 9/00 (2013.01); C21D 2211/004 (2013.01);
Abstract

A method for manufacturing Cu—Sn coexisting steel produces a good quality surface even after hot rolling. The steel is manufactured by continuous casting a molten steel that contains C: 0.04 to 0.20%, Si: 0.05 to 1.00%, Mn: 0.20 to 2.50%, P: no more than 0.05%, S: no more than 0.02%, Cu: 0.20 to 1.50%, Sn: 0.06 to 0.50%, Al: 0.06 to 1.00% and Ni: 0.05 to 1.00% by mass, and Fe and impurities as the remainder. The composition of the molten steel is defined as [Al]/(3[Si]+[Mn])≥0.050, [Ni]/([Cu]+5[Sn])≥0.10 and [Al]/[Ni]≥0.20 if the content of an element X in the molten steel is represented as [X], an internal oxidation layer is formed in a process of cooling a slab, and AlOis contained by the internal oxidation layer.