The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 17, 2018

Filed:

Jun. 06, 2014
Applicant:

Outotec (Finland) Oy, Espoo, FI;

Inventors:

Kari Valkama, Pori, FI;

Pia Sinisalo, Pori, FI;

Janne Karonen, Kokemäki, FI;

Kari Hietala, Espoo, FI;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C22B 3/08 (2006.01); C22B 3/24 (2006.01); C22B 3/44 (2006.01); C01G 3/02 (2006.01); C01G 3/05 (2006.01); C01G 3/06 (2006.01); C25C 1/12 (2006.01); C25C 1/10 (2006.01); C22B 15/00 (2006.01); C22B 3/26 (2006.01); C22B 3/00 (2006.01); C22B 3/22 (2006.01); C22B 3/46 (2006.01); C25C 1/20 (2006.01);
U.S. Cl.
CPC ...
C22B 15/0071 (2013.01); C01G 3/02 (2013.01); C01G 3/05 (2013.01); C01G 3/06 (2013.01); C22B 3/0005 (2013.01); C22B 3/08 (2013.01); C22B 3/22 (2013.01); C22B 3/24 (2013.01); C22B 3/44 (2013.01); C22B 3/46 (2013.01); C22B 11/04 (2013.01); C22B 15/0086 (2013.01); C22B 15/0089 (2013.01); C22B 15/0091 (2013.01); C25C 1/12 (2013.01); C25C 1/20 (2013.01); Y02P 10/234 (2015.11); Y02P 10/236 (2015.11);
Abstract

Provided is a method of recovering copper and one or more precious metals comprising leaching copper-bearing ore and/or concentrate under atmospheric or slightly pressurized conditions at a temperature below the boiling point of the leach solution in a sulfuric acidic solution in the presence of one or more alkali metal or alkali earth metal halides, whereby the total halide concentration is from 30 to 115 g/L, to dissolve copper and to obtain a leaching liquor comprising copper, sulfur species, and halides in solution. The leaching liquor is then subjected to a solid-liquid separation after which a first aqueous pregnant leach solution and a copper depleted leaching residue are obtained. Copper is purified by solvent extraction from the first aqueous pregnant leach solution to obtain a first copper-containing loaded organic solution and a first aqueous raffinate. The copper containing loaded organic solution is stripped and copper is recovered.